Stainless Steel Sheet/Plate 416
One of the most common alloys to undergo heat treating, 416 SS is capable of attaining the highest strength, hardness, and wear resistance of all stainless alloys. It also has excellent machinability and non-galling characteristics. 416 stainless steel is often used in parts that require extensive machining and corrosion resistance. Heat treating 416 makes it an ideal selection for cutting tools. We are suppliers of 416 stainless steel plate in 0.1875″ to 4.000″ thickness.
416 Stainless Steel Sheet/Plate, Annealed, is typically used for marine, industrial, and structural applications. 416 stainless steel offers excellent machinability, especially for a Stainless Steel alloy. Strength and corrosion resistance are lower than those of most other stainless alloys as a result.
Product Description
| Specification | 416 Stainless Steel Plate(Hot rolled, cold rolled) |
|---|---|
| Standard | ASTM A240, JIS4304 – 2005, ASTM A167, EN10088 – 2 – 2005, GB/T3280 – 2007, etc |
| Material | 201, 202, 304, 304L, 304H, 309, 309s, 316, 316L, 317, 317L, 321, 321H, 310, 347, 347H, 410, 416, 420, 430, 440, 904, 904L |
| Surface | the surface and finish of stainless steel Plate:2B, 2D, BA, NO.1, NO.4, NO.8, 8K, mirror, checkered, embossed, hair line, sandblast, Brush, etching, etc |
| Thickness | 5mm – 100mm |
| Width | 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, etc |
| Length | 2000mm, 2440mm, 3000mm, 5800mm, 6000mm, etc |
| Brand: | Kuwait Origin, European Origin, Japanese Origin, US Origin, Korea Origin, Taiwan Origin |
| Manufacturer: | POSCO, Aperam, Jindal Stainless, DKC Korea, Thyssenkrupp, Baosteel, TISCO, Arcelor Mittal, VDM, Nippon Metal, Outokumpu |
| Package | Standard export package, suitable for all kinds of transport, or as required. |
Chemistry Information
| Percentage | Si | S | C | Fe | Cr | Mo | Mn | P |
|---|---|---|---|---|---|---|---|---|
| Element | 1 max | 0.15 min | 0.15 max | 84 | 13 | 0.6 max | 1.25 max | 0.06 max |
Physical Properties 416 Stainless Steel Sheet:
| Property | Value |
|---|---|
| Density | 0.282 lb/in³ |
| Ultimate Tensile Strength | 75 ksi |
| Yield Tensile Strength | 43 ksi |
| Shear Modulus | 11,000 ksi |
| Shear Strength | 49 ksi |
| Fatigue Strength | 33 ksi |
| Hardness (Rockwell | Brinell) | B92 | 195 |
| Elongation at Break Percentage | 31% |
| Reduction of Area | 50% |
| Modulus of Elasticity | 28,000 ksi |
| Poisson’s Ratio | 0.28 |
| Machinability Percentage | 85% |
| Melting Point | 2,700-2,790 °F |
| Specific Heat | 1.1 x 10⁻¹ BTU/lb-°F |
| Thermal Conductivity | 204 BTU-in/hr-ft²-°F |
| Electrical Conductivity | 2.9% IACS |
Mechanical Properties Of 416 Stainless Steel Sheet:
| Tempering Temperature (°C) | Tensile Strength (MPa) | Yield Strength 0.2% Proof (MPa) | Elongation (% in 50mm) | Hardness Brinell (HB) | Impact Charpy V (J) |
|---|---|---|---|---|---|
| Annealed | 517 | 275 | 30 | 262 | – |
| Condition T | 758 | 586 | 18 | 248 – 302 | – |
| 204 | 1340 | 1050 | 11 | 388 | 20 |
| 316 | 1350 | 1060 | 12 | 388 | 22 |
| 427 | 1405 | 1110 | 11 | 401 | # |
| 538 | 1000 | 795 | 13 | 321 | # |
| 593 | 840 | 705 | 19 | 248 | 27 |
| 650 | 796 | 670 | 17.5 | 253 | 38 |
Application
- Gas Processing Industries
- Petrochemical industries
- Power Generation industries
- Food Processing Industries
- Chemical industries
- Oil & Gas Industries
- Fertilizers IndustriesSugar industries
Application
Agricultural Modernization
Construction Engineering
Environmental Protection Engineering
Food Processing Industry
Intelligent Home Appliances
Medical and Health Field
New Energy Infrastructure